Why do zirconia ceramics turn yellow after sintering
Why do zirconia ceramics turn yellow after sintering?
High-quality zirconia ceramics typically exhibit a white surface, while those containing impurities may appear yellow or gray. Notably, even high-purity zirconia ceramics can turn yellow after the sintering process. This discoloration phenomenon can be attributed to the following key factors:
Firstly, the use of new saggers or setter plates. Newly manufactured saggers and setter plates often retain residual volatile substances or unreacted components. Therefore, it is necessary to perform empty firing several times to remove these impurities before loading them with products for formal sintering.
Secondly, potential issues with the sintering furnace parameters. On one hand, the temperature in the high-temperature zone may exceed the optimal range for zirconia sintering; on the other hand, poor ventilation of the furnace chimney can lead to the accumulation of exhaust gases and volatile by-products, which in turn affects the surface color of the ceramics.
Thirdly, improper product stacking and inadequate oxidizing atmosphere. Excessive stacking of products during sintering will hinder the uniform circulation of the furnace atmosphere, resulting in localized oxygen deficiency. When sintering is not conducted in a sufficient oxidizing atmosphere, oxygen vacancies are likely to form in the zirconia crystal structure, and these structural defects are a major cause of yellow discoloration.
Fourthly, impurities in the raw materials and inappropriate doping levels. Iron impurities present in zirconia raw materials are prone to oxidation during the high-temperature sintering process, forming iron oxide compounds that impart a yellow hue to the ceramic surface. Additionally, excessive yttrium doping—commonly used as a stabilizer for zirconia—can also alter the material's optical properties, leading to unwanted coloration. As a practical solution, opening the furnace lid appropriately to enhance air circulation during the sintering process may significantly improve the surface color uniformity of the products.
Fifthly, contamination inside the sintering furnace. Long-term use of the furnace without regular cleaning may result in the deposition of residual impurities, volatile substances, or reaction by-products on its inner walls. These contaminants can adhere to the ceramic surface or react with it during sintering, causing yellow discoloration.
Frequently Asked Questions
Contact Us
Name: Linda Huang
Tel: +86-512-66255075
Fax: +86-512-66255030
Mobile: +86-18550512237
E-mail: [email protected]
Skype: smkceramic
MSN: [email protected]
QQ: 836574060
WeChat: 18550512237
Whatsapp: 8618550512237
Add: 11-8 Xiangshan Li,No.8 Gucun Road,Xukou Town,Wuzhong district.Suzhou City,China.